You searched for: Start Over Temperature Remove constraint Temperature Year within 10 Years Remove constraint Year: within 10 Years Subject Ferromagnetic materials Remove constraint Subject: Ferromagnetic materials Subject Materials Science and Engineering Remove constraint Subject: Materials Science and Engineering Subject Mechanical Engineering Remove constraint Subject: Mechanical Engineering

Search Results

  • 14YT alloy (Fe-14Cr-0.25wt.%Y2O3-0.4wt.%Ti) with 4 at.% Sc addition was previously reported to exhibit a nanoscale microstructure and high strength when annealed at temperatures up to 1000 °C (0.65Tm) ...